Anchor bolts

Status
Not open for further replies.

Maad

Mechanical
Joined
Jul 17, 2017
Messages
6
Location
IQ
Dear All , I need your help to choose the right material for flare riser anchor bolts ,the available materials are (S355J2 , Grade 1045 , C45R-01).The designer suggested ASTM A 307 Gr.C but its not available right now. Note that the flare riser Hight 55m and the the design wind speed 45 M/S .
 
You need to talk to the designer, and tell him his first choice material is not available.

Rise height and wind speed tell us nothing. If all you care about is structural load, it's also impossible to choose a material without knowing bolt sizes, locations, quantities, etc etc.

Your designer is the only one who can help you.
 
I suggest you read the following;


We used them for the steel stacks using hydraulic pretensioning. You need to leave sufficient gap for the extension of the bolt and the pretensioning devise. Contact them for these for the selection of pretensioning device and perhaps for the anchor bolt material, ask all the questions in your mind for the operation before hand.

Hope it helps.
 
ASCE Anchorage Design For Petrochemical Facilities, Table 2.1a Common Materials For Anchor Bolts And Studs:

A307 Grade A
A354 Gr BC
A354 Gr BD
A449

Table 2.1b Anchor Rods

A36 (F1554 Gr 36)
A193 Gr B7
A320 Gr L7
F1554 Gr 55, Gr 105


Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 