During inspection I experienced Leakage In lean amine line which is from flange side I tried to Check all ewelds by mean of Ultrasonic testing but face following difficulties,
1.Temperature of line is at higher side i.e.250 Deg F.
2.As leakage observed from flange thats why i tried to check weld/HAZ from flange side but it was not possible because area is not enough to provide access for shear wave examination.
Do any one share with me his experience regarding
1.Is this lean amine stress corrosion cracking.
2.If yes what is the best suitable method to detect this type of cracking in remaining joints of line which is working at 250 deg f.
3. iF NO THEN WHAT TYPE OF DEFECT/LEAKAGE IS THIS ALONG WITH CAUSES.
4. Is there any alternate for scanning of joints rather then Ultrasonic shear wave testing.
Looking for your cooperation
Regards
1.Temperature of line is at higher side i.e.250 Deg F.
2.As leakage observed from flange thats why i tried to check weld/HAZ from flange side but it was not possible because area is not enough to provide access for shear wave examination.
Do any one share with me his experience regarding
1.Is this lean amine stress corrosion cracking.
2.If yes what is the best suitable method to detect this type of cracking in remaining joints of line which is working at 250 deg f.
3. iF NO THEN WHAT TYPE OF DEFECT/LEAKAGE IS THIS ALONG WITH CAUSES.
4. Is there any alternate for scanning of joints rather then Ultrasonic shear wave testing.
Looking for your cooperation
Regards