Hi everyone, To pierce stainless steel from 8 mm upwards, I use the M103 A3 function (with pre-hole of 1 or 1.5 mm in diameter).
The machine performs a first piercing phase using line 103 (power 3000, hz 100, duty 25, oxygen assistance gas and 6mm nozzle height). in the second phase he performs the pre-hole and goes to use the parameters of the edge table 205 (where I can set, speed, and powers and parameters of the gas) and performs everything at a height of 1.5mm from the sheet. is it possible to change this last height?if yes , where?
The machine performs a first piercing phase using line 103 (power 3000, hz 100, duty 25, oxygen assistance gas and 6mm nozzle height). in the second phase he performs the pre-hole and goes to use the parameters of the edge table 205 (where I can set, speed, and powers and parameters of the gas) and performs everything at a height of 1.5mm from the sheet. is it possible to change this last height?if yes , where?