Co2_Marcus
Computer
hi.
can anyone say what mirror in resonator cause the sharp peak in the center.
Fanuc C4000i-B resonator.
beam mode taken at 5 meter mark.
hot mode looks good but has a sharp peak in the center. maybe 6-7mm long.
cold mode does not have this long peak.
the problem that started is that cutting with some conditions that uses full 4000watt
doesnt seem to cut trough anymore. same conditions was great a few months back on same steel.
but if cutting on lower power (3000) and slower it works.
can anyone say what mirror in resonator cause the sharp peak in the center.
Fanuc C4000i-B resonator.
beam mode taken at 5 meter mark.
hot mode looks good but has a sharp peak in the center. maybe 6-7mm long.
cold mode does not have this long peak.
the problem that started is that cutting with some conditions that uses full 4000watt
doesnt seem to cut trough anymore. same conditions was great a few months back on same steel.
but if cutting on lower power (3000) and slower it works.