Currently we have 3 large crude oil storage tanks with internal floating roofs, each has a 3' x 3' inspection hatch on the outer roof in order to look for excess oil which may have escaped and is sitting on the floating roof. The hatch itself is carbon steel which is extremely heavy. Would there be any issue of converting the steel hatch to an aluminum hatch in order to cut down on the weight of it. Could I encounter any significant problems with having two dissimilar metals in a somewhat potentially corrosive atmosphere (H2S)?