Hey Guys New Here, Trying to bend Some Tube and there is a constant failure rate happening.
Machine : BLM_Elect80
Tooling: Bend Die 3"CLR
Material :
AL - 6061 T1 OD 2" &1/2" // ID 2.37" // WT .065 Seamless Round
AL - 6063 T52 OD 2" &1/2" // ID 2.37" // WT .065 Seamless Round
AL - 5052 T0 OD 2" &1/2" // ID 2.37" // WT .065 Seamless Round
With the 6061 It was first Ordered as T6, this was to Brittle to Bend, So It snapped on first bend. Then brought down to a T1. This Process Caused the tube to Oval. Wouldn't fit on the Mandrel and thus also Caused it to Snap.
With the 6063 T52 It showed up Oval and Had Varying Wall thickness. This material was set aside , Some of it was Oval Enough to Try and out of 10 bends only two worked.
With the 5052-0 It Appears it's as well To soft or To Brittle.
It snapped on first bend as well.
Can anyone lend any Ideas to how I may fix these issues?
I have already Changed the Pressures from the bender etc...
We are Leaning towards using the 6063 T52.
Wondering If a Heating Process Before Bending is suggested or anything else?
Thank you in Advance!!!
Machine : BLM_Elect80
Tooling: Bend Die 3"CLR
Material :
AL - 6061 T1 OD 2" &1/2" // ID 2.37" // WT .065 Seamless Round
AL - 6063 T52 OD 2" &1/2" // ID 2.37" // WT .065 Seamless Round
AL - 5052 T0 OD 2" &1/2" // ID 2.37" // WT .065 Seamless Round
With the 6061 It was first Ordered as T6, this was to Brittle to Bend, So It snapped on first bend. Then brought down to a T1. This Process Caused the tube to Oval. Wouldn't fit on the Mandrel and thus also Caused it to Snap.
With the 6063 T52 It showed up Oval and Had Varying Wall thickness. This material was set aside , Some of it was Oval Enough to Try and out of 10 bends only two worked.
With the 5052-0 It Appears it's as well To soft or To Brittle.
It snapped on first bend as well.
Can anyone lend any Ideas to how I may fix these issues?
I have already Changed the Pressures from the bender etc...
We are Leaning towards using the 6063 T52.
Wondering If a Heating Process Before Bending is suggested or anything else?
Thank you in Advance!!!