I am looking for a general cost comparison for the finishing operations for aluminum alloy. The specific question I am trying to determine the answer to is: Is there a cost effective (cheaper) alternative to Anodizing aluminum alloy for which we can retain the Emissivity and thermal conductance and not have to mask off (high labor charges) grounding area's for a PCB?
1. Conversion Coatings (Iridite)
2. Anodize
3. Electroless Nickel
4. Alumniplate
5. Iridite w/ high emissivity paint
Could someone help me put these finishes (and any other I have missed) in order from least to most expensive?
Notes:
-(1,3,&4) don't have the emmisivity close to (2&5).
-5 still requires the labor to masking for holes and interior surfaces.
- I am designing a small electronic enclosure which needs to disipate about 8-10W. We are looking at ways to optimize the enclosures ability to expel heat.
Thanks in advance!
Mike
1. Conversion Coatings (Iridite)
2. Anodize
3. Electroless Nickel
4. Alumniplate
5. Iridite w/ high emissivity paint
Could someone help me put these finishes (and any other I have missed) in order from least to most expensive?
Notes:
-(1,3,&4) don't have the emmisivity close to (2&5).
-5 still requires the labor to masking for holes and interior surfaces.
- I am designing a small electronic enclosure which needs to disipate about 8-10W. We are looking at ways to optimize the enclosures ability to expel heat.
Thanks in advance!
Mike