Hai,

Anybody can answer it the Aluminu Plate(Al Mg Si 0,5) Equvalent American Standard.And also answer the preheat temerature of materail ((Al Mg Si 0,5)proir to start Aluminum Bus BAR welding.

Thanks
Sahavas
 
Replies continue below

Recommended for you

Anybody can answer it the Aluminu Plate(Al Mg Si 0,5) Equvalent American Standard.

EN 573-3 / EN AW-6060 = Al Mg Si 0,5

Equvalent American Standard : ASME/BPVC SEC II - B material SB-221 / 6060 T51/T61
look self four preheat temerature [bigglasses]
 
Generally speaking, you do not preheat aluminum or its alloys unless the surfaces are wet, damp, icy, or there is snow on the surface.

Carbon and high strength low allow, and high alloy steels may require preheat to retard the cooling rate to prevent the formation of undesirable microstructures (Martensite). That isn't the case for Austenitic stainless steels, aluminum alloys, copper, etc.


Best regards - Al
 