aluminum painting

Status
Not open for further replies.

rellimmm

Mechanical
Apr 12, 2004
1
I make aluminum tool boxes....they tarnish quickly from raod salt...what clear protective coating can i put on it, and how do i prep the aluminum.......

ty
 
Replies continue below

Recommended for you

Aluminium alloy wheels for automobiles use an acrylic powder coating to resist corrosion due to road deicing salts. This should work well for you. A typical procedure would be:

alkaline cleaning to remove oil, grease, etc.
chemical conversion coating
powder coating

Try contacting DuPont for more information:


Regards,

Cory