gsyrett725
Mechanical
We are having difficulties creating a consistent radii on our new mandrel bender. the material and 6063 T4 and the parts have about a 110mm radius and about 40mm wide x 15mm tall. it has 4 bends all 90 degrees. The part has a +- tolerance of 1mm on both the radii, length and width. We are having a hard time getting a consistent radii and it will vary from 107 to 110 in a single part. This is making it very difficult to make consistent parts. As for every mm the radius changes it effects the leg length equally.They are not staying consistent as which bend is small or large either. One time bend 1 will be perfect all other small. Next time bend 3 will be good and all others small. The angles all seem to be good within .3 degree.
Thanks in advance.
Thanks in advance.