Does anyone have parameters for cutting aluminum dross free or at least a brittle small sized dross? My company uses a 2kw Fiber Laser. Any help at all would be fantastics.
 
Replies continue below

Recommended for you

When my machine will be fixed I will give parameters. Like that I say do the samething than ss but slower
 