i am looking to buy a scanning tool for aluminum brazing, we make brazed parts and i would like to scan up to a thickness of 15mm, looking for none brazed areas,
any idea please?
 
Replies continue below

Recommended for you

ultrasonic testing (UT) equipment?. Specifically, you should look for phased array ultrasonic testing (PAUT) systems that offer high-resolution imaging and can be calibrated for aluminum.

R.Efendy
 
When once upon a time, I worked with radiographic inspection to verify braze
Penetration between joints
 