Does anyone have experience with aluminum anodes in cooling water heat exchanger channels to protect pass partition plates? Our experience with zinc anodes suggests that they are consumed too quickly. Some limited experience (second hand) suggested that aluminum anodes broke off in chunks and plugged tubes. At the time, I thought it might have to do with improper heat treatment leading to intergranular corrosion.
any comments?
any comments?