davidlight
Mechanical
- Aug 14, 2009
- 2
I took some 0.050-inch 6061-T6 sheet metal and annealed it. My intent was to bring it back to the T0 temper. I programmed the oven to go to 775F, hold temp for 1.5 hours, then reduce temp at -50F per hour until 500F is reached, with a hold time of zero. So the oven turned off after that, and the part slowly air cooled. I had some hardness tests done on the specimens, and they were so soft that they were below the lowest numbers on the charts. I have not found any treatment schedules to bring it from T0 to T6, can I just use the same treatment schedule to bring T4 to T6?