According to the ASM Handbook, here are some properties at -195 [°]C:
Sand cast test bars:
Ultimate tensile strength 275 MPa
Tensile yield strength 193 MPa
Fracture strain 0.035
Gravity die cast test bars:
Ultimate tensile strength 330 MPa
Tensile yield strength 220 MPa
Fracture strain 0.05