Hi,

Does somebody can explain to me the differnce between the 6061-T6 and the 6061-T651 ? There is one stronger or better than the other one ?

Thansk in advance.
 
Asked and answered about 1 week ago:

thread330-207831

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Status
Not open for further replies.