hI. We are currently reviewing changing the type of coating we apply to the studs OF our flanges. For many years we have installed cadmium-coated studs, which for the conditions of marine environments present excellent resistance, but for environmental and health issues, we are checking other options. Does anyone know options for a similar or superior coating?

apiexam.com
 
lubricate PTFE coated Studs - teflon

Regards
 
Google "XYLAN studs eng-tips MJ Cronin"

MJCronin
Sr. Process Engineer
 
Hot Dip Galvanised Bolting has been used for offshore environments.


*** Per ISO-4126, the generic term
'Safety Valve' is used regardless of application or design ***

*** 'Pressure-relief Valve' is the equivalent ASME/API term ***
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top