Is there an alternative to triloy alloy bars for shafting applications?
 
Replies continue below

Recommended for you

Steel?

I googled "triloy" and got references to a polycarbonate/abs alloy, i.e. plastic. Seems like just about any metal would work better?
 
Yes, is the one from wearanswers.com. Will take a look at the offer from Niagara-LaSalle, thank you!
 
The Stressproof from Niagara did not work, any other alternative?
 
Didn't work how? Size? Strength? some other issue?
Let us know what problem you are trying to solve.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
A long time ago, Stressproof didn't work for me, because I bought it to nominal size, which didn't leave enough material to clean up the 'bark'.
I should have bought Stressproof G/P to size, or regular Stressproof oversize by 1/4" or more.



Mike Halloran
Pembroke Pines, FL, USA
 
What's "Triloy"? Can you specify this? because i dont find any information about that.
 
You really need to answer Ed's question if you want more help.
 