Hey folks,
Just looking for some input on using an alternate method of welding studs to plate other than 'conventional' stud welding.
I am assuming that the stud can only be a mild steel which will limit its structural performance if it is welded to plate via a complete pen weld by pencil point or chisel point prep.
The original planned stud was a M16 Nelson stud which is comparable to A325.
thanks
DRW
Just looking for some input on using an alternate method of welding studs to plate other than 'conventional' stud welding.
I am assuming that the stud can only be a mild steel which will limit its structural performance if it is welded to plate via a complete pen weld by pencil point or chisel point prep.
The original planned stud was a M16 Nelson stud which is comparable to A325.
thanks
DRW