VIJAYANSA

Mechanical
Jul 23, 2014
17
Hi,
While calculating allowable stress value using sec II part D & code of construction is sec Viii Div 1 for SA-240 304 at 150F, it show just "-"(hyphen)only. that symbol refers to what?

Can I use that material at 150F? How can I find the allowable stress value at 150F for that material?

Regards,
Vijayan
 
Replies continue below

Recommended for you

The material is permitted at 150 deg F, the ... means the allowable stress is not reported but can be interpolated between 100 deg F and 200 deg F, which have reported values.
 
Thanks a tonne Mr. Metengr,

Did you find anything in ASME code like we can interpolate the values for that ... (Hyphen)?
 