Allowable Stress for SA-516-70

Status
Not open for further replies.

wallace24

Mechanical
Joined
May 22, 2002
Messages
16
Location
US
Hi,
Is it possible to issure a purchase order for SA-516-70 with a stated elevated min. yield strength - and be able to establish an elevated allowable stress (ie, Sa = Sy x 2/3)?
This would of course be for higher temperatures where the yield governs Sa.
Thanks.
 
Are you familar with ASME Boiler and Pressure Vessel Code allowable stress values?
 
I guess "etched in stone" and the "values" in the tables would go in the same sentence.
Thank you.
 