Hi,
Is it possible to issure a purchase order for SA-516-70 with a stated elevated min. yield strength - and be able to establish an elevated allowable stress (ie, Sa = Sy x 2/3)?
This would of course be for higher temperatures where the yield governs Sa.
Thanks.
 
Replies continue below

Recommended for you

Are you familar with ASME Boiler and Pressure Vessel Code allowable stress values?
 
I guess "etched in stone" and the "values" in the tables would go in the same sentence.