Hi,
I want to know that how much reinforcement allow for
drum to falthead welding by submerged arc welding?
Is it different for ASME SecI & Sec IV?
Pls. let me know
Mihir5577
 
do you mean flathead?
can you explain better,
you are saying flat head. which flat head on boilers?
what type of boiler?
youyr post leave many holes (nopt tube holes)...
genblr
 
Mihir,

max reinforcement is given in table PW-33, and depends on the thickness of the parent metal, and the type of weld (circf. in pipe and tube or other).

I don't know about sect IV.

swig.
 
Sec IV is more forgiving in the construction of
low pressure, I would use the same criteria construction as Sec I for the higher pressures,
since there are no rules it is safer that way,
note that some Companies even xray the long-seams in Sec IV
as well because they want to be asured of the quality,
I may do the same in the future.