Hi,

I'm trying to track down an allowable for a Nitronic (21-6-9) orbital weld. I've been told that 32% is the appropriate knockdown to apply but I'd like to find a reference that supports this. Does anyone know of anything?

Thanks much...
 
Replies continue below

Recommended for you

mathlete7;
Not enough information to answer your post. What is the application for this weld?

 