The subject says it all. Can anyone in our group give me the AISI or ASTM equivalent of this British Standard Steel.
I am pretty sure that it was originally a plate steel that was rolled into a cylinder, fabricated into a quarter or half section of a large ring gear, normalized or at least stress relieved, it was probably re-heat treated to achieve an internal hardness of approximately 325 Brinnel and then had helical gear teeth cut into it.
Any help would be greatly appreiciated.
Thanks,
teb1
I am pretty sure that it was originally a plate steel that was rolled into a cylinder, fabricated into a quarter or half section of a large ring gear, normalized or at least stress relieved, it was probably re-heat treated to achieve an internal hardness of approximately 325 Brinnel and then had helical gear teeth cut into it.
Any help would be greatly appreiciated.
Thanks,
teb1