Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

AISI 6150 Heat Treat

Status
Not open for further replies.

mfgenggear

Aerospace
Joined
Jan 23, 2008
Messages
3,611
Location
US
It would be nice if some one could share after though harden heat treat data of actual parts contraction or expansion.

We are making a hollow gear shafts about 6" long
Unfortunately, I cannot post a print because of customer proprietary issues. Through Harden Heat Treat to 44HRc.
AISI 6150 Steel

I am looking for actual inch per inch expansion or contraction.
Any issues with distortion.

Thanks
 
What is the quenchant? Are you able to provide wall thickness?
 
salt or oil (mar temper or mar quench)
 