Jun 21, 2012 #1 azzt Mechanical Joined May 19, 2004 Messages 32 Location GB Hi I'm trying to find some creep rupture data at elevated temperatures for aisi 4340 steel at conditons other than normalized (which I already have). Ideally for material around about a HRC=45. Any help would be appreciated. Thanks allan
Hi I'm trying to find some creep rupture data at elevated temperatures for aisi 4340 steel at conditons other than normalized (which I already have). Ideally for material around about a HRC=45. Any help would be appreciated. Thanks allan
Jun 21, 2012 1 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US http://deepblue.lib.umich.edu/bitstream/2027.42/4320/5/bab3992.0002.001.pdf Upvote 0 Downvote