Hi

I'm trying to find some creep rupture data at elevated temperatures for aisi 4340 steel at conditons other than normalized (which I already have). Ideally for material around about a HRC=45.

Any help would be appreciated.

Thanks

allan
 
Thanks mentengr

allan
 