Can some one suggest a source for true stress strain curves for AISI4130
at 350F.


SUMATECH, INC.
 
1. ASM Handbooks
2. Atlas of stress-strain curves
3. Graphical stress-strain plot using available end points
4. Ramberg-Osgood Equation
5. ASME Sec VIII Div 2-ANNEX 3.F/ASME Sec II Part D for equations or similar properties at high temperature
6. 7. 8. API 579

Hope it helps.
 
I would add Metallic Materials Properties Development and Standardization (MMPDS) and Aerospace Structural Materials Handbook (ASMH). Or try Google:




Rick Fischer
Principal Engineer
Argonne National Laboratory
 