Nov 19, 2018 #1 sumacon2003 Structural Joined May 3, 2005 Messages 6 Location IN Can some one suggest a source for true stress strain curves for AISI4130 at 350F. SUMATECH, INC. http://www.sumacon.com
Can some one suggest a source for true stress strain curves for AISI4130 at 350F. SUMATECH, INC. http://www.sumacon.com
Nov 19, 2018 1 #2 NRP99 Mechanical Joined Jan 21, 2016 Messages 483 Location IN 1. ASM Handbooks 2. Atlas of stress-strain curves 3. Graphical stress-strain plot using available end points 4. Ramberg-Osgood Equation 5. ASME Sec VIII Div 2-ANNEX 3.F/ASME Sec II Part D for equations or similar properties at high temperature 6. http://asm.matweb.com/search/SpecificMaterial.asp?bassnum=m4130r7. https://icme.hpc.msstate.edu/mediawiki/index.php/Stress_Strain_data-4130_Steel8. API 579 Hope it helps. Upvote 0 Downvote
1. ASM Handbooks 2. Atlas of stress-strain curves 3. Graphical stress-strain plot using available end points 4. Ramberg-Osgood Equation 5. ASME Sec VIII Div 2-ANNEX 3.F/ASME Sec II Part D for equations or similar properties at high temperature 6. http://asm.matweb.com/search/SpecificMaterial.asp?bassnum=m4130r7. https://icme.hpc.msstate.edu/mediawiki/index.php/Stress_Strain_data-4130_Steel8. API 579 Hope it helps.
Nov 19, 2018 #3 rickfischer51 Mechanical Joined Jun 27, 2013 Messages 453 Location US I would add Metallic Materials Properties Development and Standardization (MMPDS) and Aerospace Structural Materials Handbook (ASMH). Or try Google: https://ntrs.nasa.gov/archive/nasa/casi.ntrs.nasa.gov/19630001179.pdf https://icme.hpc.msstate.edu/mediawiki/index.php/Stress_Strain_data-4130_Steel http://dspace.library.iitb.ac.in/jspui/bitstream/10054/1456/1/5256-1.pdf Rick Fischer Principal Engineer Argonne National Laboratory Upvote 0 Downvote
I would add Metallic Materials Properties Development and Standardization (MMPDS) and Aerospace Structural Materials Handbook (ASMH). Or try Google: https://ntrs.nasa.gov/archive/nasa/casi.ntrs.nasa.gov/19630001179.pdf https://icme.hpc.msstate.edu/mediawiki/index.php/Stress_Strain_data-4130_Steel http://dspace.library.iitb.ac.in/jspui/bitstream/10054/1456/1/5256-1.pdf Rick Fischer Principal Engineer Argonne National Laboratory