May 9, 2007 #1 1handle Electrical Joined Feb 3, 2006 Messages 6 Location US Dear peers, Does anybody know, where to get AISI 405 stainles steel BH curve, please? Thank you.
May 10, 2007 #2 MagMike Materials Joined Jun 4, 2003 Messages 506 Location US I'm not aware of a curve for that material, it is not processed for its magnetic properties. If you are willing to spend the money, there are testing houses that'll measure it for a nominal fee. Upvote 0 Downvote
I'm not aware of a curve for that material, it is not processed for its magnetic properties. If you are willing to spend the money, there are testing houses that'll measure it for a nominal fee.
Jun 28, 2007 #3 RMWS Electrical Joined Jun 28, 2007 Messages 4 Location US My laboratory can measure B,H curves on magnetic materials. Let me know if we can help out. KJS Associates. Magnetic Instrumentation, Inc. http://www.maginst.com Upvote 0 Downvote
My laboratory can measure B,H curves on magnetic materials. Let me know if we can help out. KJS Associates. Magnetic Instrumentation, Inc. http://www.maginst.com