In the AISC 16th manual, page 16.1-131, Table J2.5, the second-to-last heading box gives the load type and direction relative to weld axis as:

"Tension or compression - parallel to weld axis"

The available strength listed for this case is:

"Tension or compression in parts joined parallel to a weld is permitted to be neglected in design of welds joining the parts."

What in the world does this mean? How can I just neglect the load in the parts when designing the weld? What load do I design the weld for then? I will probably need a picture/sketch to understand what's going on here...

Thanks in advance!
 
Loads parallel to weld axis are mainly borne by the constituent parts themselves. The weld itself doesn't really do much to resist sigma_parallel (see below picture).