AISC 360-16 Hole Diameter

Status
Not open for further replies.

Struct-007

Structural
Aug 7, 2020
32
In the 15th Edition of the Steel Manual, I noticed the following discrepancy:

Table J3.3 in AISC 360-16 shows that the Standard hole diameter of a 1 inch bolt is (1-1/8").
Table 3.1 in RCSC-14 shows that the Standard hole diameter of a 1 inch bolt is (1-1/16").

Which value should we consider?
 
Replies continue below