What affect and how much can the temperature of rubber prior to molding have on the results of the molded parts on an injection press? For example if the room you are running a mold in is 55°F one day and the next day it is 70°F, how will this affect the results of the parts being made if all other factors are the same such as the settings on the press/mold?