Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Adhesively Bonded Composite Joint Analysis

Status
Not open for further replies.

Burner2k

Aerospace
Joined
Jun 13, 2015
Messages
193
Location
IN
Hi folks,
I am attempting to learn on performing a static linear (for time being) stress analysis of an adhesive bonded laminate joint. I decided to do a 3D analysis since I am interested in through the thickness stresses in the adhesive layer. Since this is the first time I am attempting the above, I wanted to have my bdf file checked for potential errors. The software I am using is Femap v11.2.2.

FYI, I was able to run the analysis without errors. But I wanted some feedback on definition of 3D solid laminate element in Femap/NX Nastran. Let me provide some info which may be required. The composite laminate (doubler) is 0.0741" thick and consists of 13 plies. While modeling the doubler in FE, I chose 2 solid elements through the thickness. I learnt later that Nastran just takes the total thickness of the laminate from PCOMP definition and allots all the plies to one solid element i.e. if I have 2 solid elements through the thickness, then I may require 2 different layups & 2 solid properties to get the correct layup orientation & thickness. This is what I have done. I hope I am correct here.

Anyways, I am posting some excerpts of the bdf file here and appreciate any thoughts on the same. Thanks in advance

PARAM,POST,-1
PARAM,OGEOM,NO
PARAM,AUTOSPC,YES
PARAM,K6ROT,100.
PARAM,GRDPNT,0
CORD2C 1 0 0. 0. 0. 0. 0. 1.+FEMAPC1
+FEMAPC1 1. 0. 1.
CORD2S 2 0 0. 0. 0. 0. 0. 1.+FEMAPC2
+FEMAPC2 1. 0. 1.
$ Femap with NX Nastran Coordinate System 3 : Doubler Lay Up Coord
CORD2R 3 0 0. 0. .01 0. 0. 1.01+
+ 7.8246-7 1. .01

$ Femap with NX Nastran Property 1 : Aluminum Skin 0.08in Thk
PSOLID 1 1 0
$ Femap with NX Nastran Property 2 : Potting
PSOLID 2 2 0
$ Femap with NX Nastran Property 3 : Adhesive 0.01in Thk
PSOLID 3 3 0
$ Femap with NX Nastran Property 4 : Doubler Bottom
PCOMPS 4 3 13 14100. 14100. 0. 0. +
+ 1 4 .0057 -45. YES +
+ 2 4 .0057 45. YES +
+ 3 4 .0057 -45. YES +
+ 4 4 .0057 45. YES +
+ 5 4 .0057 90. YES +
+ 6 4 .0057 0. YES +
+ 7 4 .00285 0. YES
$ Femap with NX Nastran Property 5 : Doulber Top
PCOMPS 5 3 13 14100. 14100. 0. 0. +
+ 8 4 .00285 0. YES +
+ 9 4 .0057 0. YES +
+ 10 4 .0057 90. YES +
+ 11 4 .0057 45. YES +
+ 12 4 .0057 -45. YES +
+ 13 4 .0057 45. YES +
+ 14 4 .0057 -45. YES
$ Femap with NX Nastran Material 1 : 2024-T3 Sheet Bare
MAT1 1 1.05+7 .33 .1 0. 0.
$ Femap with NX Nastran Material 2 : Potting
MAT1 22400000. .41 0. 0. 0.
$ Femap with NX Nastran Material 3 : Adhesive
MAT1 3 319000. .32 0. 0. 0.
$ Femap with NX Nastran Material 4 : Composite Tape
MAT11 4 2.83+72700000.2700000. .21 .019 .21 914000.+
+ 914000. 750000. .0723 0. 0. 0. 0.
 