Dear mates,
A coating contractor has applied a HEMPEL epoxi (NOVOLAC)coating of high solids at erratic DFT 300/500 µm and adhesion test values also erratic 5/8 Mpa (100% adhesive failure), which would be a normally acceptable adhesion value for this product and DFT.
Thanks for any input.