https://www.southwire.com/wire-cable/bare-aluminum-overhead-transmission-distribution/acsr/p/ALBARE6Aluminum Conductor, Steel Supported. (ACSS)
Construction
- Aluminum 1350-H19 wires, concentrically stranded about a steel core. Standard core wire for ACSR is class A galvanized
- Class A core stranding is also available in zinc-5% aluminum-mischmetal alloy coating.
- For aluminum-clad (AW) ACSR, please refer to the ACSR/AW catalog sheet
- Additional corrosion protection is available through the application of grease to the core or infusion of the complete cable with grease
https://apar.com/wp-content/uploads/2021/02/4.-Aluminium-Conductor-Composite-Core-ACCC.pdfAluminum Conductor Composite Core Conductors (ACCC): These are "High-temperature low-sag" (HTLS) Conductors with excellent electrical characteristics, excellent sag-tension characteristics and superior corrosion resistance to that of ACSR. As compared to ACSR they have lighter weight, comparable strength and current carrying capacity, lower electrical losses and superior corrosion resistance have given this conductor wide acceptance as a transmission conductor. It has found limited use, however, as a distribution conductor.
Construction
Fully annealed trapezoidal shaped aluminum wires concentrically stranded over hybrid carbon and glass fiber core (Composite Core)
ACSS is really a fine choice. It is even better using trapezoidal wire. I appreciate what ACCC brings to the table but wow, why would you want to run a conductor that hot? Just because it performs thermally doesn't mean you won't have voltage issues, clamp issues, and terminal issues while cooking your ACCC wire at high temperatures.Logical reason to jump from ACSR to ACCC without considering ACSS? Currently utilizing 477 ACSR on 69 line and being pushing to jump to ACCC without considering any ACSS options.