Mar 23, 2010 #1 wagnermj Chemical Joined Mar 17, 2010 Messages 15 Location US I am in need of a standard(s) where I can find specific visual acceptance criteria for ductile iron valve bodies.
I am in need of a standard(s) where I can find specific visual acceptance criteria for ductile iron valve bodies.
Mar 25, 2010 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Review ASTM A 395. Upvote 0 Downvote