Well if you don't invoke your own spec then that is what you will get.
There are companies that I know of that require multiple CI specs so that both chemistry and properties get constrained.
On the other hand if you are getting the desired properties why would you care about chemistry?
It is only CI.
= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed