Stated Parameters
(a)A practical question: could the magnetic field in a VIM cause iron contamination (pick-up) from the iron particle residuals (from previously iron-based melt) on the melting chamber?
Depends on particle size and rate of heating.
(b)VIM=vacuum inducting melting, the power level is high at 100KW. The frequency is actually about 1000Hz, the polarity change is such quick, not sure the solenoid coil can attract any ferromagnetic subject.
Here again paricle size is important, due to skin depth and rate it temperature increase
(c) the polarity change in ferromagnetic materials can be up to microwave range. In a typical FeCoB/Mgo/FeCoB STT-MRAM, magnetization switch is up to 10GHz. however, the spinning of magnetic moment or domain movement doesnot seem to mean it will exert a force. Even in doorbell case, if the distance between teh plunger and the chime is twice as large, could the back-and-forth forces, generated by the solenoid, be canceled out?
With microwave range drive field, switching not likely with metal particulates, more likely just heating, which for small paricles results in results in rapid temperature changes.