Hi!
We seem to be having an issue with a customer who complains that some of the ABS in their products is starting to "bubble". After cutting the product through the raised area, it appears that it is only the ABS and not the Elastopor foam that has expanded.
We supply the same products to other customers who don't complain about this issues. Is there anything that they might be doing that would cause this problem. Photos below.
Many thanks!
Jack