I didn't paste all the input file. Below is the complete input file:
*Heading
Axial load
** Job name: Force Model name: Model-1
*Preprint, echo=NO, model=NO, history=NO, contact=NO
**
** PARTS
**
*Part, name="Soft nanoneedle"
*Node
1, -500., 350., 10000.
2, -500., 500., 10000.
3, -500., 350., 9500.
4, -500., 500., 9500.
5, -500., 350., 9000.
6, -500., 500., 9000.
7, -500., 350., 8500.
8, -500., 500., 8500.
9, -500., 350., 8000.
10, -500., 500., 8000.
11, -500., 350., 7500.
12, -500., 500., 7500.
13, -500., 350., 7000.
14, -500., 500., 7000.
15, -500., 350., 6500.
16, -500., 500., 6500.
17, -500., 350., 6000.
18, -500., 500., 6000.
19, -500., 350., 5500.
20, -500., 500., 5500.
21, -500., 350., 5000.
22, -500., 500., 5000.
23, -500., 350., 4500.
24, -500., 500., 4500.
25, -500., 350., 4000.
26, -500., 500., 4000.
27, -500., 350., 3500.
28, -500., 500., 3500.
29, -500., 350., 3000.
30, -500., 500., 3000.
31, -500., 350., 2500.
32, -500., 500., 2500.
33, -500., 350., 2000.
34, -500., 500., 2000.
35, -500., 350., 1500.
36, -500., 500., 1500.
37, -500., 350., 1000.
38, -500., 500., 1000.
39, -500., 350., 500.
40, -500., 500., 500.
41, -500., 350., 0.
42, -500., 500., 0.
43, -330., 350., 10000.
44, -330., 500., 10000.
45, -330., 350., 9500.
46, -330., 500., 9500.
47, -330., 350., 9000.
48, -330., 500., 9000.
49, -330., 350., 8500.
50, -330., 500., 8500.
51, -330., 350., 8000.
52, -330., 500., 8000.
53, -330., 350., 7500.
54, -330., 500., 7500.
55, -330., 350., 7000.
56, -330., 500., 7000.
57, -330., 350., 6500.
58, -330., 500., 6500.
59, -330., 350., 6000.
60, -330., 500., 6000.
61, -330., 350., 5500.
62, -330., 500., 5500.
63, -330., 350., 5000.
64, -330., 500., 5000.
65, -330., 350., 4500.
66, -330., 500., 4500.
67, -330., 350., 4000.
68, -330., 500., 4000.
69, -330., 350., 3500.
70, -330., 500., 3500.
71, -330., 350., 3000.
72, -330., 500., 3000.
73, -330., 350., 2500.
74, -330., 500., 2500.
75, -330., 350., 2000.
76, -330., 500., 2000.
77, -330., 350., 1500.
78, -330., 500., 1500.
79, -330., 350., 1000.
80, -330., 500., 1000.
81, -330., 350., 500.
82, -330., 500., 500.
83, -330., 350., 0.
84, -330., 500., 0.
*Element, type=C3D8R
1, 43, 44, 46, 45, 1, 2, 4, 3
2, 45, 46, 48, 47, 3, 4, 6, 5
3, 47, 48, 50, 49, 5, 6, 8, 7
4, 49, 50, 52, 51, 7, 8, 10, 9
5, 51, 52, 54, 53, 9, 10, 12, 11
6, 53, 54, 56, 55, 11, 12, 14, 13
7, 55, 56, 58, 57, 13, 14, 16, 15
8, 57, 58, 60, 59, 15, 16, 18, 17
9, 59, 60, 62, 61, 17, 18, 20, 19
10, 61, 62, 64, 63, 19, 20, 22, 21
11, 63, 64, 66, 65, 21, 22, 24, 23
12, 65, 66, 68, 67, 23, 24, 26, 25
13, 67, 68, 70, 69, 25, 26, 28, 27
14, 69, 70, 72, 71, 27, 28, 30, 29
15, 71, 72, 74, 73, 29, 30, 32, 31
16, 73, 74, 76, 75, 31, 32, 34, 33
17, 75, 76, 78, 77, 33, 34, 36, 35
18, 77, 78, 80, 79, 35, 36, 38, 37
19, 79, 80, 82, 81, 37, 38, 40, 39
20, 81, 82, 84, 83, 39, 40, 42, 41
*Nset, nset=_PickedSet2, internal, generate
1, 84, 1
*Elset, elset=_PickedSet2, internal, generate
1, 20, 1
** Region: (NeedleSection

icked)
*Elset, elset=_PickedSet2, internal, generate
1, 20, 1
** Section: NeedleSection
*Solid Section, elset=_PickedSet2, material=Silicon
1.,
*End Part
**
**
** ASSEMBLY
**
*Assembly, name=Assembly
**
*Instance, name="Soft nanoneedle-1", part="Soft nanoneedle"
*End Instance
**
*Nset, nset=_PickedSet4, internal, instance="Soft nanoneedle-1"
41, 42, 83, 84
*Elset, elset=_PickedSet4, internal, instance="Soft nanoneedle-1"
20,
*Nset, nset=_PickedSet5, internal, instance="Soft nanoneedle-1"
1, 2, 43, 44
*Elset, elset=_PickedSet5, internal, instance="Soft nanoneedle-1"
1,
*Nset, nset=_PickedSet6, internal, instance="Soft nanoneedle-1"
1, 2, 43, 44
*End Assembly
**
** MATERIALS
**
*Material, name=Silicon
*Elastic
1e-07, 0.3
**
** BOUNDARY CONDITIONS
**
** Name: Fixed Type: Displacement/Rotation
*Boundary
_PickedSet4, 1, 1
_PickedSet4, 2, 2
_PickedSet4, 3, 3
_PickedSet4, 4, 4
_PickedSet4, 5, 5
_PickedSet4, 6, 6
** Name: Pinned Type: Displacement/Rotation
*Boundary
_PickedSet5, 1, 1
_PickedSet5, 2, 2
** ----------------------------------------------------------------
**
** STEP: Apply load
**
*Step, name="Apply load", perturbation
Axial load
*Buckle
6, , 12, 30
**
** BOUNDARY CONDITIONS
**
** Name: Fixed Type: Displacement/Rotation
*Boundary, op=NEW, load case=1
_PickedSet4, 1, 1
_PickedSet4, 2, 2
_PickedSet4, 3, 3
_PickedSet4, 4, 4
_PickedSet4, 5, 5
_PickedSet4, 6, 6
*Boundary, op=NEW, load case=2
_PickedSet4, 1, 1
_PickedSet4, 2, 2
_PickedSet4, 3, 3
_PickedSet4, 4, 4
_PickedSet4, 5, 5
_PickedSet4, 6, 6
** Name: Pinned Type: Displacement/Rotation
*Boundary, op=NEW, load case=1
_PickedSet5, 1, 1
_PickedSet5, 2, 2
*Boundary, op=NEW, load case=2
_PickedSet5, 1, 1
_PickedSet5, 2, 2
**
** LOADS
**
** Name: Force Type: Concentrated force
*Cload
_PickedSet6, 3, -1.
**
** OUTPUT REQUESTS
**
*Restart, write, frequency=0
**
** FIELD OUTPUT: F-Output-1
**
*Output, field, variable=PRESELECT
*End Step