Well, I was testing quickly how is co-simulation working on an example last week. I succeeded runing it but still a lot to do in order to get what I really want but if it helps, here you go:
.inp for CDF:
*Surface, type=ELEMENT, name=_PickedSurf7, internal
__PickedSurf7_S4, S4
__PickedSurf7_S6, S6
__PickedSurf7_S5, S5
__PickedSurf7_S3, S3
*Elset, elset=_PDF_WholeModel, internal, instance=Fluid-1, generate
1, 13298, 1
*End Assembly
**
** MATERIALS
**
*Material, name=Material-1
*Density
1e-09,
*Expansion
0.0008,
*Specific Heat, type=CONSTANTPRESSURE
4.21e+06,
**
** PREDEFINED FIELDS
**
** Name: Predefined Field-1 Type: Fluid density
*Initial Conditions, type=Density
_PDF_WholeModel, 1e-09
** Name: Predefined Field-2 Type: Fluid thermal energy
*Initial Conditions, type=TEMPERATURE, Element Average
_PDF_WholeModel, 300.
** ----------------------------------------------------------------
**
** STEP: Step-1
**
*Step, name=Step-1
*CFD, incompressible navier stokes, energy equation=TEMPERATURE
0.01, 0.3, 0.025, 0.45, 1
1e-10, 0.5, , , 0.5
*Momentum Equation Solver
50, 2, 1e-05
*Pressure Equation Solver
250, 2, 1e-05
ICC, 1, 1, CG
*Transport Equation Solver
50, 2, 1e-05
**
** BOUNDARY CONDITIONS
**
** Name: BC-1 Type: Fluid inlet/outlet
*Dsload
_PickedSurf5, P, 16.
*Dsload
_PickedSurf5, TEMP, 300.
** Name: BC-2 Type: Fluid inlet/outlet
*Dsload
_PickedSurf6, P, 0.
** Name: BC-3 Type: Fluid wall condition
*Dsload
_PickedSurf7, VELX, 0.
_PickedSurf7, VELY, 0.
_PickedSurf7, VELZ, 0.
**
** LOADS
**
** Name: Load-1 Type: Gravity
*Dload
, GRAV, 9810., 0., -1., 0.
** Interaction: Int-1
*Co-simulation, name=Int-1, controls=Int-1_Ctrls, program=MULTIPHYSICS
*Co-simulation Region, import, type=SURFACE
_PickedSurf4, TEMP
*Co-simulation Region, export, type=SURFACE
_PickedSurf4, HFL
*Co-simulation Controls, name=Int-1_Ctrls, coupling scheme=gauss-seidel, time incrementation=lockstep, time marks=yes,
step size=min, scheme modifier=lag
**
** OUTPUT REQUESTS
**
*Restart, write, frequency=0
**
** FIELD OUTPUT: F-Output-1
**
*Output, field
*Node Output
DENSITY, PRESSURE, TEMP, TURBNU, U, V
*Output, history, frequency=0
*End Step
.inp for standard:
**
** MATERIALS
**
** SA182 Gr F304 or 316
** SA351 Gr CF8A or CF8M
*Material, name=Austenitic_High_Alloy_Steel_COL
*Conductivity
14.5, 21.11
14.5, 37.78
15., 65.56
15.4, 93.33
15.8, 121.11
16.2, 148.89
16.5, 176.67
17., 204.44
17.3, 232.22
17.7, 260.
18.1, 287.78
18.5, 315.56
18.9, 343.33
19.2, 371.11
19.6, 398.89
20., 426.67
20.4, 454.44
20.7, 482.22
21.1, 510.
21.5, 537.78
22., 565.56
22.3, 593.33
22.7, 621.11
23., 648.89
23.5, 676.67
23.9, 704.44
24.2, 732.22
24.6, 760.
24.9, 787.78
25.4, 815.56
*Density
7.92e-09, 21.11
7.91784e-09, 37.78
7.91421e-09, 65.56
7.91055e-09, 93.33
7.90686e-09, 121.11
7.90314e-09, 148.89
7.8994e-09, 176.67
7.89564e-09, 204.44
7.89186e-09, 232.22
7.88805e-09, 260.
7.88423e-09, 287.78
7.88038e-09, 315.56
7.87651e-09, 343.33
7.87263e-09, 371.11
7.86872e-09, 398.89
7.86479e-09, 426.67
*Elastic
209601., 0.3, -198.33
206153., 0.3, -128.89
202706., 0.3, -73.33
195122., 0.3, 21.11
190985., 0.3, 93.33
186848., 0.3, 148.89
183401., 0.3, 204.44
179953., 0.3, 260.
175127., 0.3, 315.56
170990., 0.3, 371.11
166164., 0.3, 426.67
*Expansion
1.64e-05, 21.11
1.65e-05, 37.78
1.67e-05, 65.56
1.68e-05, 93.33
1.69e-05, 121.11
1.7e-05, 148.89
1.72e-05, 176.67
1.73e-05, 204.44
1.74e-05, 232.22
1.75e-05, 260.
1.76e-05, 287.78
1.77e-05, 315.56
1.78e-05, 343.33
1.79e-05, 371.11
1.8e-05, 398.89
1.81e-05, 426.67
*Specific Heat
4.7201e+08, 21.11
4.7592e+08, 37.78
4.8178e+08, 65.56
4.8743e+08, 93.33
4.9334e+08, 121.11
4.9933e+08, 148.89
5.0696e+08, 176.67
5.1069e+08, 204.44
5.185e+08, 232.22
5.2428e+08, 260.
5.2786e+08, 287.78
5.3347e+08, 315.56
5.3928e+08, 343.33
5.447e+08, 371.11
5.5058e+08, 398.89
5.5394e+08, 426.67
** SA182 Gr F304 or 316
** SA351 Gr CF8A or CF8M
*Material, name=Austenitic_High_Alloy_Steel_COL_sup
*Conductivity
14.5, 21.11
14.5, 37.78
15., 65.56
15.4, 93.33
15.8, 121.11
16.2, 148.89
16.5, 176.67
17., 204.44
17.3, 232.22
17.7, 260.
18.1, 287.78
18.5, 315.56
18.9, 343.33
19.2, 371.11
19.6, 398.89
20., 426.67
20.4, 454.44
20.7, 482.22
21.1, 510.
21.5, 537.78
22., 565.56
22.3, 593.33
22.7, 621.11
23., 648.89
23.5, 676.67
23.9, 704.44
24.2, 732.22
24.6, 760.
24.9, 787.78
25.4, 815.56
*Density
7.92e-09, 21.11
7.91784e-09, 37.78
7.91421e-09, 65.56
7.91055e-09, 93.33
7.90686e-09, 121.11
7.90314e-09, 148.89
7.8994e-09, 176.67
7.89564e-09, 204.44
7.89186e-09, 232.22
7.88805e-09, 260.
7.88423e-09, 287.78
7.88038e-09, 315.56
7.87651e-09, 343.33
7.87263e-09, 371.11
7.86872e-09, 398.89
7.86479e-09, 426.67
*Elastic
209601., 0.3, -198.33
206153., 0.3, -128.89
202706., 0.3, -73.33
195122., 0.3, 21.11
190985., 0.3, 93.33
186848., 0.3, 148.89
183401., 0.3, 204.44
179953., 0.3, 260.
175127., 0.3, 315.56
170990., 0.3, 371.11
166164., 0.3, 426.67
*Expansion
1.64e-05, 21.11
1.65e-05, 37.78
1.67e-05, 65.56
1.68e-05, 93.33
1.69e-05, 121.11
1.7e-05, 148.89
1.72e-05, 176.67
1.73e-05, 204.44
1.74e-05, 232.22
1.75e-05, 260.
1.76e-05, 287.78
1.77e-05, 315.56
1.78e-05, 343.33
1.79e-05, 371.11
1.8e-05, 398.89
1.81e-05, 426.67
*Specific Heat
4.7201e+08, 21.11
4.7592e+08, 37.78
4.8178e+08, 65.56
4.8743e+08, 93.33
4.9334e+08, 121.11
4.9933e+08, 148.89
5.0696e+08, 176.67
5.1069e+08, 204.44
5.185e+08, 232.22
5.2428e+08, 260.
5.2786e+08, 287.78
5.3347e+08, 315.56
5.3928e+08, 343.33
5.447e+08, 371.11
5.5058e+08, 398.89
5.5394e+08, 426.67
**
** INTERACTION PROPERTIES
**
*Surface Interaction, name=Contact_COL_COLsup
1.,
*Friction, slip tolerance=0.005
0.3,
*Surface Behavior, no separation, pressure-overclosure=HARD
*Gap Conductance
15., 0.
0., 0.01
*Surface Interaction, name=Contact_COLsup_ShimPlate
1.,
*Friction, slip tolerance=0.005
0.3,
*Surface Behavior, pressure-overclosure=HARD
*Clearance, master=COL-1.OUT, slave=COL_sup-3.Contact_COL, value=0.
*Clearance, master=COL-1.OUT, slave=COL_sup-4.Contact_COL, value=0.
**
** BOUNDARY CONDITIONS
**
** Name: BC-3 Type: Displacement/Rotation
*Boundary
_PickedSet13, 2, 2
_PickedSet13, 3, 3
** Name: BC-4 Type: Displacement/Rotation
*Boundary
_PickedSet14, 2, 2
_PickedSet14, 3, 3
**
** PREDEFINED FIELDS
**
** Name: Predefined Field-4 Type: Temperature
*Initial Conditions, type=TEMPERATURE
COL-1.Complete, 30.
**
** INTERACTIONS
**
** Interaction: COL_COLsup3
*Contact Pair, interaction=Contact_COL_COLsup, small sliding, type=SURFACE TO SURFACE
COL_sup-3.Contact_COL, COL-1.OUT
** Interaction: COL_COLsup4
*Contact Pair, interaction=Contact_COL_COLsup, small sliding, type=SURFACE TO SURFACE
COL_sup-4.Contact_COL, COL-1.OUT
** ----------------------------------------------------------------
**
** STEP: Step-10
**
*Step, name=Step-10, inc=1000
*Heat Transfer, end=SS, deltmx=30.
0.3, 0.3, 3e-06, 0.3, 0.0002
** Interaction: Int-6
*Co-simulation, name=Int-6, controls=Int-6_Ctrls, program=MULTIPHYSICS
*Co-simulation Region, import, type=SURFACE
COL-1.IN, CFL
*Co-simulation Region, export, type=SURFACE
COL-1.IN, NT
*Co-simulation Controls, name=Int-6_Ctrls, coupling scheme=gauss-seidel, time incrementation=subcycle, time marks=yes,
step size=min, scheme modifier=lead
**
** OUTPUT REQUESTS
**
*Restart, write, frequency=0
**
** FIELD OUTPUT: F-Output-2
**
*Output, field
*Node Output
NT,
*Contact Output
PPRESS,
*Output, history, frequency=0
*End Step
I didn't paste geometry or assemblies...
Hope it helps.