What tests are required to qualify a PQR for welding A706 Gr60 reinforcing bars to a P8 stainless steel plate to be used as an embed in concrete. All welding will be performed in the flat position.
 
Replies continue below

Recommended for you

This typically falls under the jurisdiction of AWS D1.4. It will outline the required qualifications based on joint geometry and a number of other variables.
 