If welding a588 that is going to be exposed, bare weathered, multi pass groove with E8XTX A5.29 filler metal for atmosheric corrosion and weathering characteristics, can this be done with a pre-qualified wps?
A558 is a group II material, therefore can you write a wps just for A588 welded with 80 series filler or would you have to produce a pqr?Table 4.5 PQR essential variable changes - filler metal 1) Increase in filler metal classification strength.
BUT, Table 3.1, A588 with note b Special welding material and WPS(e.g. E80XX-X low alloy electrodes) may be required ect. ect.
So does that mean that you can write a WPS prequalified to meet the requirement, or does a PQR need to be performed, I'm a little stumped...
Thanks for advice/comments,Robert
A558 is a group II material, therefore can you write a wps just for A588 welded with 80 series filler or would you have to produce a pqr?Table 4.5 PQR essential variable changes - filler metal 1) Increase in filler metal classification strength.
BUT, Table 3.1, A588 with note b Special welding material and WPS(e.g. E80XX-X low alloy electrodes) may be required ect. ect.
So does that mean that you can write a WPS prequalified to meet the requirement, or does a PQR need to be performed, I'm a little stumped...
Thanks for advice/comments,Robert