Does anyone have the Densities of A53, A36, 304SST & 316SST Steels?

Thanks,

CADArt
 
All listed above would be approximately 0.28 lbs/in3 at ambient temperature.
 
How close do you need them.
All plain steels are roughly 0.283 lb/cu in (7.84 g/cc3)
For 304 I use 0.285 (7.9)
And for 316 0.287(7.95)

You need a ref book.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 