The A36 is 10" pipe, eventaully having the id hardfaced. I dont see any prior purging of the interior of the pipe required in the past. I am working with a new fabricator...just welded up his test coupon..be it a pipe coupon...gtaw process for the root pass 309L...smaw process using flux cored sticks 309L for the fill and cap...no purge...he was not impressed with the visual aspects of the coupon but sent it out for evaluation anyways....he mentioned the possiblity of purging the pipe..lot of purge gas. This is code welding. Bob