Dec 20, 2007 #1 laquinnia Structural Joined Dec 20, 2007 Messages 2 Location US I have a "low" temperature application for structural steel. The design temperature is about -60F. Are A325 bolts suitable at this temperature or must I go to A320 bolts?
I have a "low" temperature application for structural steel. The design temperature is about -60F. Are A325 bolts suitable at this temperature or must I go to A320 bolts?
Dec 20, 2007 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US This is considered low temperature service, and I would use A 320 material. Upvote 0 Downvote