Hi,

Whithout any specific service what are the restriction to made PWHT to A216WCB(pump casing) after welding nozzles.

thks in advance
 
If you have no Code of Construcction, follow good engineering practice - -

1" or greater weld deposit thickness, PWHT at 1100 deg F - 1 hour/inch of weld deposit thickness.
 