I saw a valve part specification like this.

"Key: Carbon steel, A108-1045"

But you can't find 1045 in ASTM A108.

So I think this is a customry notation, combined with ASTM and AISI. Then, if want to know about this material, what publication do I have to look up?


 
Replies continue below

Recommended for you

AISI no longer maintains any standards for steel chemical composition. ASTM and SAE do. Section 7 of ASTM A 108 lists the applicable references for chemical compositions. ASTM A 29 is the probably the most common reference for ASTM A 108, since it defines the requirements for the hot-rolled bars that are turned into cold-finished bars according to ASTM A 108. Grade 1045 appears in ASTM A 29.
 
SAE 1045; "NOTE 3—A more complex ordering description is as follows: Steel Bar; ASTM A 108, dated ____; SAE 1045; Fine Grain; Cold Drawn, Turned, Ground and Polished; chamfer both ends; Mechanical Property Test Results; Hardness test; 2.000-in. (50.80 mm) diameter round; 12 ft
(3657.61 mm) long; Heat Analysis ..."
 